I'm building 36' fiberglass Spray by Roberts Bruce.
Currently I'm working on deck and cabin top. My plan says that deck and top cabin supposed to be sandwich method (2CSM+18WR+2CSM+5/8"Balsa+2CSM+18WR+2CSM). Side cabin it is 6 layers of fiberglass solid. I did changes to this schedule. I built deck using 0.75" marine plywood and side cabin 0.75" marine plywood as well. I make this decision because I want to put any hardware on deck wherever I want. I did ask Bruce about new fiberglass schedule over the plywood but unfortunately I didn't get clear answer because it is against his recommendation. I'm planning to cover the plywood by 2 layers of 18WR mostly because I have a lot of left over. On cabin top I'm going to keep sandwich method. Any suggestion about fiberglass schedule over 0.75" plywood deck? Thanks for any help in advance. Adam For direct e-mail use |
#2
![]() |
|||
|
|||
![]()
My deck, cabin side and cabin top are of 2 layers of 1/2" ply and I glassed
mine using a fab-mat that had a chopped strand on the face of the roving. I would recommend that you lay a layer of CSM at the same time you lay your 18WR as a binder. Much the same as when you doing a glass lay up. The 18WR being rather course weave. -- My opinion and experience. FWIW Steve s/v Good Intentions (Ingrid 38) |
#3
![]() |
|||
|
|||
![]()
Thanks Steve - Actually I got this idea from your website and your pictures.
Scotty - you are absolutely right. I'm getting this problem many times. OK - here you a CSM - Chopped Strand Mat 2CSM it is 2 oz per square foot WR - Woven Roving 18WR it is 18 oz per square yard How it looks? - take a look here i.e. http://www.noahsmarine.com/Canada/Fi...glass-can.html BTW it is my supplier - for my project. Thanks Adam |
#4
![]() |
|||
|
|||
![]()
"Adam" wrote in message ...
Thanks Steve - Actually I got this idea from your website and your pictures. Scotty - you are absolutely right. I'm getting this problem many times. OK - here you a CSM - Chopped Strand Mat 2CSM it is 2 oz per square foot WR - Woven Roving 18WR it is 18 oz per square yard How it looks? - take a look here i.e. http://www.noahsmarine.com/Canada/Fi...glass-can.html BTW it is my supplier - for my project. Thanks Adam Thanks Adam, I appreciate being answered without the attitude of the OG... ![]() Scotty |
Reply |
Thread Tools | Search this Thread |
Display Modes | |
|
|
![]() |
||||
Thread | Forum | |||
fiberglass pontoon leak on boat slip, HELP! | General | |||
New Deck | General | |||
Replacing Wood Deck | General | |||
Varnishing a house deck? [deck refinishing] | General | |||
Varnishing a house deck? [deck refinishing] | Boat Building |